Logo Museum
Museum
Friends of Durham Mining Museum
Events Calendar
e-Books and Books for sale
Photograph Gallery
Document Archive
Main Document Archive
Newspaper Articles
Articles by date
Articles by colliery
Personal name index
Local Record Extracts
D.M.A. Document Archive
Transactions of I.M.E.
Miners' Welfare
N.C.B. Archive
The Colliery Engineer
The Colliery Guardian
Mine & Quarry Engineering
Mining Journal
The Science and Art of Mining
Coal Magazine
Coal News
Coke and Gas
Master Name Index
What's new in the site
Mining
Mining History
Colliery Index
Colliery Maps
Company Overviews
Who's Who
Mineral Information
Managers Certificates
Educational Material
Bibliography
Statistics
Workers/Employee Lists
Notes for Family Historians
War Service information
Disasters
Disaster Reports
Names of those killed
Disasters in the 1700s
Disasters in the 1800s
Disasters in the 1900s
Memorials
Awards for Gallantry
On this day ...

Links to other sites of interest
Industrial Heritage Days Out
Former www.pitwork.net web site

Index to site

Contact and address details

Share Page with Social Media

Share on Facebook

Share with Reddit

Share on Delicious


 Newspaper Articles Index Newspaper Articles 

25th January 1941, Page: 228, Column: 1

Effects Of Weathering On Mineral Matter

The paper on "The Storage of Coal: Effects without Rise in Temperature," read before the South Staffordshire and Warwickshire Institute of Mining Engineers, dealt in particular with investigations on Coleford Highdelf coal, in which the summary and interpretation were reproduced in No. 13 (pages 193-4) of this journal. The authors of the paper — Messrs. Frank Scarf, Douglas A. Hall, and Cecil W. Yearsley — also discussed the effects of weathering on mineral matter, and the appended notes from this section of the paper may suitably be studied as a contribution to the extracts already submitted.

Loss of carbon dioxide during weathering is a process mainly determined by the preliminary oxidation of pyrites to iron sulphate and sulphuric acid. The loss of carbon dioxide is thus mainly due to a secondary chemical reaction occurring in the mineral matter, and its rate is independent of the oxidation of the coal substance. The loss of carbonate from the 1/400 to 0 inch fraction which has been weathered in a small bag Was very much less than that from the equivalent fraction intermixed with larger sizes of the pearls. At the end of the year the carbon dioxide content of the former had fallen from 2.62 to 2.33 per cent., while the intermixed fraction had fallen to 1.46 per cent. As a result of degradation some ankerite and pyrites is detached from the larger pieces of coal and may have an important effect on the carbonate and sulphur contents of the fine sizes, e.g., the transfer of only 0.01 per cent, of carbonate from the larger fractions of pearls to the 1/400 to 0 inch fraction would result in an increase of about 1 per cent. in the carbonate content of the latter. It is probable, therefore, that the loss of carbonate from the finest fractions is even more rapid than is indicated by the results. Oxidation of pyrites, loss of carbonate, and finally lixiviation of sulphates will be initiated in this order, but afterwards these reactions will proceed simultaneously until all the pyrites is oxidised. The percentage of sulphates may therefore vary greatly during the process of weathering. Total sulphur contents fall at the same rate as that at which sulphates are removed, and are unaffected by sulphate formation ; conversely, pyritic sulphur contents fall at the same rate as that at which sulphates are formed, and are unaffected by sulphate removal. This statement is based on the fact that the results obtained in this work indicate that organic sulphur percentages remain constant during weathering, which conforms with the general opinion.

The total sulphur content of doubles remained sensibly constant. On the other hand, in both sets of pearls there was a gradual and constant loss, totalling in the case of the dump pearls about 0.3 per cent, during the 2½ years. The fall in pyritic sulphur of the pearls was somewhat more rapid than the fall in total sulphur. As in the case of carbonate, there was some difference in the behaviour of the respective fractions of the two sets of pearls in regard to sulphur changes. It may be noted that the 1/400 to 0 inch fraction of sack pearls first increased from 4.1 to 4.4 per cent. total sulphur in six months, and in the second six months fell to 4.0 per cent. It appears that increase in mineral matter is the main factor in this fraction. This is supported by the constancy of the sulphur content of the equivalent fraction kept in a small bag, in which accumulation is impossible and leaching-out apparently did not occur until the exposed sample had been reduced to very small bulk. It was noticed that this sample formed a clot which was presumably comparatively impervious to air. The largest particles of this fine coal have a diameter of the order of 0.06 mm., and Rosin has shown that with coal as large as 0.1 to 0.25 mm. the whole of the voids can be filled with adherent moisture. In the dump pearls the coarse fractions down to 1/80 inch lost sulphur at the same rate as that for the sack pearls, but below this size increases were found.

Sulphate sulphur percentages indicated very slight oxidation of the pyrites in the doubles over two years. The fractions of sack pearls down to 1/80 inch showed no appreciable change in one year. Finer fractions showed increases, but these fractions were present in such small proportions that changes in their composition did not appreciably affect the composition of the pearls as a whole. The increases found in these fractions were progressively greater with smaller particle size. Dump pearls showed more rapid oxidation of pyrites to sulphate than sack pearls, not only as a whole but also in the corresponding fractions. The general conclusion is that inorganic sulphur is gradually removed from the coal as a whole ; from fine fractions it is dissolved more rapidly, but at the same time these fractions gain sulphur by accumulation from the coarser fractions. The graph of pyritic sulphur contents shows that all the fractions would contain some 0.5 per cent. of pyritic sulphur after about four years.

No change is discernible in the total percentage of mineral matter of the doubles during 2½ years. The pearls fell somewhat in mineral content, the dump pearls from about 11.2 to a mean value for the five final samples of 10.3 per cent. This loss was borne out by the values found in the constituent fractions. Presumably it was due mainly to evolution of carbon dioxide during the reaction between carbonates and pyrites in oxidising conditions, and the subsequent leaching-out of sulphates.

In the absence of leaching the result of the reaction, in so far as the mineral matter of the coal is concerned, is a gain in weight. From the recorded loss of carbon dioxide in the dump pearls, 0.64 per cent., it can be calculated that the gain in weight was 0.23 per cent. The extent to which the calcium sulphate was removed by leaching can similarly be calculated from the recorded loss (0.30 per cent.) in sulphur as 1.28 per cent. There was, therefore, a net calculated loss of 1.05 per cent., a figure agreeing well with that found experimentally, 0.9 per cent, as mentioned above. The fractions above 1/16 inch in sack pearls lost mineral matter ; the finer fractions gained mineral matter to such an extent as just to counterbalance the loss from the coarser. In the dump pearls the division between the gaining and losing fractions fell at approximately 1/80 inch. These effects confirm the theory already advanced as to the accumulation of mineral matter in fine coal. The finest fractions showed considerable increases in mineral matter, e.g., the 1/400 to 0 inch fraction of sack pearls increased from 29.2 to 48.5 per cent, in a year. The initial and final mineral contents of the fractions have been graphed against specific surface area ; thus four curves are obtained, two for each set of pearls. In the dump pearls the transfer of mineral matter from coarse to fine fractions was more extensive than in sack pearls ; moreover, the transferred mineral matter was concentrated into a narrower range of fine fractions. This may be regarded as a later stage in the process, as the dump pearls were weathered for a longer time than the sack pearls,


Names mentioned in this article

 

 Name  Age  Occupation  Notes 
Hall, Douglas A.      
Scarf, Frank      
Yearsley, Cecil W.      


 

mail
Mail:
Webmaster
Back
Back
Home
Home
Open Government Licence   Contains public sector information licensed under the Open Government Licence v3.0.

Copyright © 1999-2024 by The Durham Mining Museum and its contributors
Registered Charity No: 1110608
Page last updated: 28 Nov 2022

Privacy Policy
 
Terms & Conditions
 
Search
Search
Print
Print