24th August 1940, Page: 58, Column: 2 Causes Of Rope DeteriorationUnder this caption in last issue (page 36) the views of Mr. W. B. Carlson were quoted from the Journal of the South African Institution of Engineers. Further contributions to the discussion are being presented to the Institution, and Mr. G. W. Sharp, a past-president, expresses himself as being in favour, as far as possible, of stripping from the subject of winding ropes unnecessary doubts and seeming, and of removing the tendency to surround it with mystery and unnecessary complication. Voluminous statistics, most of them quite incomplete in those essentials necessary to form opinion, serve, as he sees it, only to obscure the issue and confuse the mind. After all, the modern winding rope is in a class where quality and consistency of manufacture is of a very fine order. It is, in fact, not so much the rope which should occasion concern as the conditions under which it works, and if we see to it that those conditions have due attention and that it is provided with a suitable factor of safety at the point at which the greatest demand is made on its strength, as well as elsewhere, we shall have done all that is necessary to safeguard the position. Taking the practical view of this subject, Mr. Sharp says the main causes of deterioration can be summed up in the three following classes (a), (b) and (c) :— (a) Abrasion, plastic deformation of the material, nicking and corrosion. (b) Bending and crushing. (c) Kinetic stress fatigue. The first group (a) is catered for by the undoubted careful attention of the operating engineer, and the effect of each cause can be easily located. Bending (b) is approximately equal in effect at all points in the rope so affected and this, together with crushing, is taken care of by the well-known standards which determine sheave and drum proportions and wire diameters. Kinetic stress fatigue (c) is the basic consideration which should govern the factor of safety and, for all practical purposes — all normal variations of alternating stress and vibration notwithstanding — it can be regarded as directly and simply proportional to the work done by the rope as between one point in its length and another. It can thus be reduced to very simple terms. Mr. Sharp proceeds to say :— Fatigue, as such, has no standard of positive measurement, but relative values can be established in terms of a common measure. Now, the degree of stress fatigue at any point in the rope will be proportional to the kinetic stresses which accompany alternating waves and general vibration, and to the number of times these stresses occur. Also, the stresses are proportional to the tension at any point, and the number of times they occur at any point is proportional to the distance travelled by that point. That is to say, knowing that the kinetic stress at any point is proportionate to the tension which contributes to it; that the number of stress repetitions is proportionate to distance travelled and that fatigue is proportionate to both, it follows that, for all practical purposes, the product of tension and distance travelled is proportionate to stress fatigue. Therefore, if we know the foot-tons expressing the product of tension and distance travelled at any point in the rope, we have the relative value of fatigue at that point, and it follows that the point at which these foot-tons are a maximum will be the point suffering the greatest fatigue from the causes under (c). Hence the statement that "the maximum shaft work done by a winding rope expressed in foot-tons is a relative measure of the fatigue to which it is subjected from stress, vibration, etc."
|
|||||||||||||||||||
![]() |
||||||||
|
Mail: Webmaster |
Back |
Home |
Copyright © 1999-2024 by The Durham Mining Museum and its contributors Registered Charity No: 1110608 Page last updated: 28 Nov 2022
|
Search |
|
|||