20th February 1943, Page: 200, Column: 2
Boiler Cracks
Mr. T. Henry Turner, M.Sc, believes that whatever the true theoretical
explanations may be of the various types of cracks which occur in boilers,
many, if not all, of the cracks could be avoided if engineers would round off
sharp edges and leave the surface of the metal in a state of compression. In
his paper on "Corrosion of Boiler Tubes" before the Institution of
Mechanical Engineers he said that cracks grow when opened out in tension. If
the surface of the steel is put into a state of compression by, for example,
heavy shot-blasting, the fatigue strength of the surface is increased, pores
are closed up, and sharp edges are rounded off. If boiler plates, after bending
and drilling, were heavily shot-blasted, especially round drilled holes, very
little would be heard about caustic or other cracking. It thus appears that a
good case can be made out both for the light shot-blasting of tubes and for the
heavy shot-blasting of the inside of a boiler shell.
 |
 |
|