Logo Museum
Museum
Friends of Durham Mining Museum
Events Calendar
e-Books and Books for sale
Photograph Gallery
Document Archive
Main Document Archive
Newspaper Articles
Articles by date
Articles by colliery
Personal name index
Local Record Extracts
D.M.A. Document Archive
Transactions of I.M.E.
Miners' Welfare
N.C.B. Archive
The Colliery Engineer
The Colliery Guardian
Mine & Quarry Engineering
Mining Journal
The Science and Art of Mining
Coal Magazine
Coal News
Coke and Gas
Master Name Index
What's new in the site
Mining
Mining History
Colliery Index
Colliery Maps
Company Overviews
Who's Who
Mineral Information
Managers Certificates
Educational Material
Bibliography
Statistics
Workers/Employee Lists
Notes for Family Historians
War Service information
Disasters
Disaster Reports
Names of those killed
Disasters in the 1700s
Disasters in the 1800s
Disasters in the 1900s
Memorials
Awards for Gallantry
On this day ...

Links to other sites of interest
Industrial Heritage Days Out
Former www.pitwork.net web site

Index to site

Contact and address details

Share Page with Social Media

Share on Facebook

Share with Reddit

Share on Delicious


 Newspaper Articles Index Newspaper Articles 

11th July 1942, Page: 4, Column: 1

Preservation Of Timber

In a paper before the Chemical, Metallurgical and Mining Society of South Africa, on "The Preservation of Timber and Fabrics with reference to Utilisation Underground," read by Mr. J. W. Bowen, M.Sc, of the Timber Research Laboratory of the Transvaal Chamber of Mines, it was pointed out that when timber is attacked by wood-destroying fungi several changes occur. (1) There is a gradual loss in weight due to hydrolysis of the carbohydrates, a series of intermediate products being produced until ultimately carbon dioxide and water are formed ; (2) there is a corresponding loss in strength ; and (3) there is a corresponding depletion of certain chemical constituents of the timber. As far as the mines are concerned these changes are particularly important, because they affect mining practice in a number of ways.

Regarding the preservation of timber Mr. Bowen said :— In order to preserve timber against fungal and insect attack, a preservative is applied which is poisonous or repellent to these organisms. Preservatives can be divided into three groups : (1) Oil preservatives, e.g., creosote, coal tar and creosote derivatives ; (2) Water-soluble preservatives, e.g., zinc chloride, copper sulphate, sodium fluoride and various arsenical preservatives ; (3) Oil-soluble preservatives, e.g., copper naphthenate, copper oloate and copper stearate and barium salts of the same acids.

The perfect preservative has yet to be discovered. It should be cheap, safe, odourless, stainless and permanent.

All types of preservatives mentioned have both advantages and disadvantages when used for the preservation of mining timber. Generally, all oil-soluble and oil preservatives can be excluded on account of cost. It must be realised that the effective life required from timber underground to a great extent governs the cost and the efficacy of treatment that can be given. Untreated timber, under conditions conducive to decay, i.e., temperatures of 80°F. and relative humidities of 95 per cent., becomes so rotten that it loses its effectiveness as support after a period of a year. By comparison, in stopes where large quantities of timber are used, rarely is a life of more than four years required from timber, consequently a cheap, relatively effective preservative is all that is wanted to give this extra life. In drives, haulages and permanent ways where considerably longer life is required, it is essential that a more effective treatment, entailing greater absorption of preservative, be given. The treatment of shaft sets is a somewhat different problem. Here an extremely long life is required from this timber and it is profitable to use a relatively costly preservative to ensure that the required life is obtained. Unfortunately excellent preservatives, e.g., creosote, have some disadvantages such as an unpleasant smell, being dirty to handle and inflammable. Whether or not these disadvantages outweigh the increase in life obtained is a moot point.

In addition a number of water-soluble preservatives cannot be considered on account of some individual disadvantages. The arsenicals are excellent preservatives, but are unsafe for natives to handle and would present a grave problem in a case of fire underground. Copper salts are also excluded as treatment is carried out in iron cylinders and precipitation of the copper results.

The present preservative used by the mining industry is a mixture of zinc sulphate from the reduction works and triolith — one of the Wolman salts — composed of sodium fluoride, potassium dichromate and dinitropbcnol. Although no cases of dermatitis have been recorded, it is advisable to take precautions and see the persons handling this salt wash and avoid unnecessary contact as the dinitrophenol is extremely poisonous.

In the method of treating timber, investigations carried out have revealed that a number of factors play an important part in the penetration and absorption of preservative into timber. Briefly these factors are as follows :—

(1) Up to air pressures of 110 lb. per square inch absorption of preservative increases correspondingly with the pressure.

(2) Most of the preservative is absorbed within the first five minutes. Continued treatment, however, increases the quantity of preservative absorbed. On being subjected to pressure for twenty minutes, timber absorbs 82 per cent. of the preservative which it would absorb if subjected to the same pressure for one hour.

(3) The temperature of the treatment solution in the case of relatively easily impregnated woods has little effect on increased absorption.

(4) Dry timber absorbs more preservative than green timber. On the sap drying out from green timber the pores become filled with air which is readily replaceable with preservative.

(5) Drawing a vacuum prior to the application of pressure brings about a considerable increase in absorption of preservative. Generally, drawing a vacuum prior to the application of pressure, treating air-dried wood only and applying maximum air pressure available for a reasonable time, are conducive to better absorption and penetration of preservative.


Names mentioned in this article

 

 Name  Age  Occupation  Notes 
Bowen, J. W.    Transvaal Chamber of Mines  


 

mail
Mail:
Webmaster
Back
Back
Home
Home
Open Government Licence   Contains public sector information licensed under the Open Government Licence v3.0.

Copyright © 1999-2024 by The Durham Mining Museum and its contributors
Registered Charity No: 1110608
Page last updated: 28 Nov 2022

Privacy Policy
 
Terms & Conditions
 
Search
Search
Print
Print