4th June 1938, Page: 378, Column: 1
Spontaneous Heating
By J. H. Bailey.
From paper read on 21st May before the North Staffordshire
Colliery Under-managers' Association.
Spontaneous heating of coal is chiefly due to the absorption of
oxygen, or oxidation. This results in the generation of heat;
if the heat is carried away as fast as it is generated, there will be
no rise in temperature. If the heat is not carried away, the rate
of oxidation increases until ignition temperature is reached.
When iron pyrites are present in the coal, they oxidise and
swell, thus breaking up the coal, exposing a greater surface to
oxidation.
The depth of the seam and the method of working it will
influence the amount of crush on the coal.
The greater the pressure, the more small coal is made, and a
larger surface area is exposed to oxidation.
When coal is being crushed, heat is generated.
The deeper the seam, the higher will be the temperature, and the
greater will be the rate of oxidation.
The larger the quantity of air circulating, the greater will be
the cooling action. The pressure required to convey the air
through the workings will influence leakage through the wastes;
therefore, the lower the pressure, the smaller will be the leakage.
By maintaining good airways and putting in good packs, the
desired quantity of air can be conveyed with a minimum pressure.
The roof in the vicinity of faults is generally very bad and
broken; falls of roof occur, resulting in crushed coal being left.
The broken ground admits air leakage, which creates oxidation.
The presence of timber and paper is dangerous, due to the
fact that these have a lower ignition temperature than coal.
Where Heatings May Occur.
Heatings occur in breaks in the coal pillars left unworked
forming the roadway supports. These breaks are caused by roof
pressure, especially where the pillars are left too small. These
breaks sometimes form a communication between intake and
return airways, and are full of fine slack, due to crush. The air
pulls through to the return, creating oxidation.
When a fall occurs at the coal face it is sometimes better to
re-open the face by cutting through the coal, leaving a rib of coal
to support the broken roof. This coal, sometimes due to bad
conditions, is left in the gob. Roof pressure comes on and grinds
the coal into slack; air percolates through the crushed coal,
causing oxidation.
Coal left adjacent to faults is usually of inferior quality, very.
friable and sometimes damp. The roof is usually weak and
broken. The coal, if left, is subject to excessive roof pressure.
For these reasons, heating often occurs in the vicinity of faults.
In gobs, where coal forms the roof, the crushing and grinding
of the roof creates quantities of fine slack; also where a bed of
coal forms the floor, the floor is subject to upheaval. This grinds
the floor coal into slack, also causing floor breaks. Through
these breaks air short-circuits, causing oxidation.
In packs which contain slack, inferior coal and timber, aiso
where the packing is insufficiently done (enabling the air to short
circuit through), heat will generate.
Where posts are left in the gob they cause uneven settlement
of the roof, causing leakage through the gob; also in packs they
prevent uniform settlement of the roof and the proper solidification
of the pack, allowing air leakage.
Inflammable vapour is given off timber at 163°C. and timber
ignites at about 250°C. where coal ignites at about 300°C., so
where timber is left in wastes and packs we get fire much sooner.
Detection of Spontaneous Heating.
Sweating is usually one of the first practical indications of a
heating taking place. It consists of unusual deposition of moisture
on the roof, floor and sides. The moisture appears as beads of
water, or a film of water on the pack walls. The rise in temperature,
due to heating, evaporates moisture. The hot air and gases
are given off into the air-current; here they meet with the cooler
surfaces, thus lowering the temperature and depositing the moisture.
Smell. — As the heating advances a peculiar smell is given off,
known as "gob stink," which is a sure sign that a heating is
taking place. As the heating progresses, as indicated by the
rise in temperature, there is a difference in the smell. The ability
to distinguish the different smells, at the different stages of the
heating, is of considerable practical value.
The first stage may be described as a sour smell or one of
fermentation, and as the heating progresses we get a petrol or
tarry smell. This develops until it is irritating to the nose. The
appearance of smoke is soon followed by actual fire.
Train workmen to the dangers of spontaneous combustion.
Encourage them to be on the alert for any indications where
they are working and to report the same.
Train all officials in the detection of early indications.
A fire may occur in a coal pillar any time during the first squeeze
or settlement of the roof, but after this the risk of fire diminishes,
until a fresh occurrence of the squeeze is set up.
Time depends on the liability of the material to oxidation,
the rate of air leakage, the rate at which the heat produced is
dissipated, and the remoteness of the seat of the heating. These
factors govern the interval of time between the first indications
and actual fire. Where the heating is remote very little time
elapses between the first indication and actual fire.
Prevention of Heatings.
The method of working must be: (a) Able to extract all the coal.
(b) No roadside pillars. (c) Keep the working face in a straight
line — no steps. (d) Judicious splitting of the air-current. (e)
Maintenance of large airways. (f) Prevention of access of air
to the gobs.
A method of precaution practised in North Staffordshire is to
short-circuit the air-current off the gobs and allow them to charge
up with firedamp, thus creating a non-oxidising atmosphere
where nothing can live. The danger of this method is that,
between fresh air and the inert gob, we have a belt of firedamp
and air at its most explosive mixture.
Where conditions are favourable a method to be adopted,
where the workings are to the dip, is to drive to the boundary,
working up-bank and leaving the waste behind to fill up with
water, if water is available.
The longwall method of working is favourable in the prevention
of heating, due to features already mentioned.
The seam should be divided into a number of districts, each
district having its own separate air split. The districts should
not be too large. The faces should advance at a uniform rate.
The number of roadways should be reduced to a minimum. All
roads should be packed off.
Where practical the packs should be buried, by lifting the
roadways. The construction of packs is a matter of importance
at all times. They should be constructed to prevent breakage
of the roof and prevent air-leakage, also to allow uniform subsidence
and solidification.
Where practical, complete stowage should take place, as this
reduces the breakage of the roof and the formation of cavities
where firedamp can accumulate. Should a fire occur, complete
stowage produces conditions which are safer, and the operation
of dealing with the fire is more successful. In some cases cross
packs are built to seal off the wastes. For this method to be
successful the roof must be capable of solidifying the pack, without
being broken.
Precautions with Respect to Ventilation. — (1) Ventilating splits
should be small and independent. (2) Airways should be large.
(3) Intake and return should be as far apart as possible. (4) The
difference of pressure should be as low as possible. (5) No
restriction for the air-current at the coal face. (6) Loss of air
at doors should be avoided. (7) All stoppings and air-crossings
should be airtight. (8) Preparatory stoppings should be fixed in
suitable positions for sealing off quickly. (9) All visible breaks
should be filled with stone dust. (10) Air-crossings should be
constructed in the solid.
Dealing with Heatings.
Loading Out the Fire. — Loading out can only be attempted
where the position of the heating is definite and not very large.
Desirable conditions are: Fire must be in the initial stage; Very
accessible, close to the roadside; Good roof; Free from firedamp;
A plentiful supply of water.
If the heating is close to a roadside in a pillar or a pack, water
under pressure may be applied until the heated material is
sufficiently cooled, then it can be loaded out in iron tubs and sent
to the surface. When the whole of the heated material is loaded
out, the cavity is filled with sand or flue dust — stone dust
preferable.
A retaining wall of bricks and mortar is built along the side of
the pack or pillar so as to prevent re-entry of air. This is banked
up and rammed with sand.
When loading out a fire it is essential that there shall be an
intake and return, so that work can be carried out on the intake
side of the fire and the hot and poisonous gases be carried into
the return.
Water must he plentiful when used, because if a limited supply
is used water gas is formed. Water gas is a mixture of hydrogen
and carbon monoxide, steam in contact with incandescent coal,
the hydrogen separates from the oxygen. The oxygen takes up
with the carbon from the coal and forms carbon monoxide. Here
we create an atmosphere of CO and H2 which is poisonous and
highly explosive when mixed with air.
Organisation of the men to load out the fire is very important.
There must be sufficient men to work in relays, for very short
periods, and a plentiful supply of soothing drinks.
Sealing Off. — Where the heating is inaccessible or has got a
good start, in an advanced stage, sealing off the district or a
portion of it is resorted to. As a rule this is a rush job, and if
preparatory stoppings are in a good, quick stopping is put in ;
if not, temporary stoppings have to be erected. The sites for
these must be in the solid ground, free from breaks in roof and
floor.
These stoppings may consist of two or three posts set across
the roadway; these are boarded across or old ventilation doors
fixed against the posts. This arrangement is strengthened with
bags of flue dust or send, the joints between the bags being made
with loose sand or flue dust.
A sampling pipe is fixed in the stoppings, fitted with a valve.
These stoppings must be airtight to prevent air getting to the
fire, also to retain the products of combustion to extinguish it.
When stoppings are being put in the ventilation is gradually
reduced and firedamp soon accumulates, so intake and return
stoppings must be built simultaneously and as speedily as possible,
every effort being made to synchronise the final sealing. These
can then be strengthened up as required. The sampling pipe
should always be long enough outbye to permit of this, otherwise
any disturbance of this pipe may lead to leakage into the sealed-off
area.
 |
 |
|
Names mentioned in this article
|
 |
 |
| Name | Age | Occupation | Notes |
| Bailey, J. H. | | | |