21st April 1928, Page: 316, Column: 1 News and NotesReplying to discussion at the Northern Section of the Coke Oven Managers' Association, Dr. R. Lessing said that the reason why some coals had dusts which showed some coking power — though not comparable with clean coal — was that the amount of clarain and vitrain fractions was rather higher than in others which were almost entirely fusain and clay dust. At the same time, the problem of cleaning that dust was a very difficult one on account of the very fine grades of it.
|
|||||||||||||||
![]() |
||||||||
|