At Rive de Gier on the Loire, the usual produce of Coke is found to amount to 69 per cent. of the Coal employed, and even the inferior varieties, which are there subjected to the coking process, afford from 60 to 65 per cent. of Coke, whilst in the mound process from 45 to 50 per cent. only is obtained, and in the heap, even rich Coal rarely yields more than from 40 to 45 per cent. The furnace used is constructed on the same principle as an ordinary baking oven, and consists of a flat arched space with an even floor. Like those before described, it is without a distinct fire-place, and the heat retained by the walls of the furnace or kiln after the withdrawal of one charge is sufficient to cause the ignition of that which succeeds it. The floor of this oven is an oval space, 11½ feet by 23 feet, composed of a bed of fire-clay 6 inches in thickness, spread out and well beaten on a layer of loose stones. This, again, rests on a mass of rubbish and gravel, with which the centre of the foundation is made up, and which forms the immediate support of the bottom of the furnace. For the purpose of charging and drawing the Coke, two openings are placed opposite each other at the extremity of the lesser axis of the furnace; these are closed by doors 2 feet high, and 2 feet 8 inches wide, made of iron lined with fire-bricks. Each of these door-ways is provided with cast iron linings made with grooves, in which the doors slide when raised or lowered by means of the chains and levers to which they are attached. In each of these doors is a small opening, through which the workmen can observe what is going on inside the furnace, and thereby regulate the process. The greatest distance from the roof to the floor is 4 feet. A small chimney, 1 foot 6 inches diameter, and 1 foot 5 inches in height, is placed in the centre of the dome for the escape of freed gases.
The whole of the internal lining, except the floor, is composed of fire-bricks, and the arch jointed with fire-clay. The outside of the furnace may be of either common brick or stone, but should be covered with a good layer of mortar mixed with sharp sand, for the purpose of excluding the air which might otherwise enter through the jointings of the work. Should any crack occur during the process of carbonisation, it is for the same reason carefully stopped with clay kept prepared for that purpose. The furnace is charged whilst still hot from the preceding charge, and the layer of Coal-dust, which is about 10 inches in thickness, should be evenly spread on the floor by iron rollers. The fine Coal is slightly sprinkled with water before heating; and, if it be of a very coking description, the layer on the bottom of the furnace should not exceed 8 inches in thickness. During the first two hours after charging, the doors are entirely closed, with the exception of a small slit at the bottom which allows just sufficient draught to carry off to the chimney the large quantities of gases and vapours which escape from the charge. This stage of the operation corresponds to the sweating period of the charcoal mound, and it is found that the more slowly and regularly this is conducted, the larger is the amount of Coke produced.
The charge of one of these ovens varies from 60 to 70 cubic feet, according to the more or less coking nature of the Coals. At the expiration of 2 hours after charging, the quantities of inflammable gases given off are much increased. After a short time these, mixing with the atmospheric air entering beneath the door, suddenly ignite with a sort of explosion, and the yellow smoke which has hitherto been evolved through the aperture in the dome is quickly replaced by a cloud of a much darker colour. At this point the charge is at a cherry-red heat, and it becomes necessary to increase the temperature, in order to expel the last traces of volatile matter. This is done by raising the door about 3 inches — admitting more air upon the charge — which yields an increased quantity of dusky-coloured smoke; but the smoke gets clearer and less sooty, the heat of the charge becomes uniform in all parts of the furnace, and begins to split into large columnar fragments. At this stage of the operation the doors are made close. The heat, which is, as it were, shut up in the walls, will now be sufficient to complete the charring of the Coals, and the expulsion of the last traces of gaseous matters. After thus shutting up the furnace, the flame issuing from the central chimney still flickers for a short time over the opening, but gradually becomes more and more feeble, until it finally dies away altogether. The top of the chimney is now closed by an iron plate, and the Coke drawn with as little delay as possible, in order to prevent loss of heat before the introduction of another charge of Coal, and also to retain the largest amount of fixed matter — Carbon — as its destruction goes on then rapidly. Each operation requires 24 hours for its completion, and as soon as the Coke is drawn, it is sprinkled with water, for the double purpose of cooling it more rapidly, and also of producing the decomposition of the sulphur compounds which might otherwise be retained and render the Coke of less value as a fuel. When one charge is withdrawn another is placed in the furnace, and the process goes on without intermission until it is necessary to allow the oven to cool for the purpose of examining its refractory lining, which, if made of good bricks, will require to be repaired about once in six months.
In South Wales the furnace Coals are less bituminous; they contain more carbon, and a shorter period is required for carbonisation — 24 hours for the complete operation being generally the most approved time. But by far the largest proportion of Coke used in the Welsh blast furnaces is made from hard large Coal in open beds, such Coal weighing from 31 to 32 lbs. the cubic foot, procured generally in the vicinity of the furnaces, and subject, consequently, to but little expense for carriage. From the short period required for carbonisation, a better yield is obtained, and as regards the number of ovens more work is turned out. The heat is kept up to a higher temperature by reason of these quickly repeated operations, and the necessarily short intervals of the charges, which conduces greatly to the promotion of rapid and good results, both in respect of quality and the percentage yield. Coke, however, made from the best bituminous Coals of the Durham Coalfield are, no doubt, much preferred for iron furnaces, where the expense of carriage does not amount to a prohibition; and the large quantities of Coke exported from the counties of Durham and Northumberland show the preference given to it in foreign countries.
Of recent years the manufacture of Coke has become a branch of colliery business of great importance; and, as an article of commerce, is mainly in. the hands of proprietors whose Coal is adapted for coking purposes. In many instances a Coalowner cannot find a market for his small Coal at any price; when, therefore, the Coal is suitable for being converted into Coke, one of the first considerations must be to select a suitable site for an establishment; when it can be done, the best place will be near the pit producing the Coal.
As most of the large coking collieries have to depend for their vend rather upon Coke than. Coal, any calculation made to
Please Note: These web pages retain the original pagination from the publication